Mems Group, I'm looking for a good thermal conductive glue that will bond two silicon wafers together - and be release after a few operation that require good thermal conductivity, vacuum compatible, temperature range between -20 to 125 C. Thanks, Greg Miller KVH Industries Email: gmiller@kvh.com