durusmail: mems-talk: thermal conductive glue
thermal conductive glue
2003-01-23
2003-01-23
2003-01-23
2003-01-24
2003-01-24
2003-01-23
2003-01-27
thermal conductive glue
Oray Orkun Cellek
2003-01-23
Dear Greg,

Nice question, and a trivial guess : Maybe Apiezon T or Apiezon H
(www.apiezon.com) grease can be applied.  Good thermal conductivity,
mid-temperature range, vacuum compatible & sticky I guess!  May be removed
with a solvent but I don't have any experience in that.

The only problem is : How to apply on Si wafer ?

Regards,

Oray Orkun Cellek
o.o.cellek@ieee.org
Research Assistant, Ph. D. Student
Electrical & Electronics Engineering Department
Middle East Technical University
06531 Ankara
Turkey
Tel : +90 312 210 4579
Fax : +90 312 210 1261


----- Original Message -----
From: "Greg Miller" 
To: "General MEMS discussion" 
Sent: Thursday, January 23, 2003 4:02 PM
Subject: [mems-talk] thermal conductive glue


> Mems Group,
>
> I'm looking for a good thermal conductive glue that will bond two silicon
wafers together - and be release after a few operation that require good
thermal conductivity, vacuum compatible, temperature range between -20 to
125 C.
>
> Thanks,
>
> Greg Miller
> KVH Industries
> Email: gmiller@kvh.com
>
> _______________________________________________
> MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/


reply