Hi Greg
the temperature range is pretty wide. I use some white wax from Aremco.
But the melting point is near 60 C. Maybe they have others!

http://www.aremco.com

Greetings
Stefan

_____________________________________________________
Dr. Stefan Blunier
ETH Zuerich, Zentrum CLA G 21.2
Institut fuer Mechanische Systeme
Tannenstrasse 3
CH - 8092 Zuerich
Switzerland

Tel:   +41 1 632 77 64
Fax:  +41 1 632 11 45
e-mail: blunier@imes.mavt.ethz.ch
__________________________________________________


-----Original Message-----
From: Greg Miller [mailto:gmiller@kvh.com]
Sent: Donnerstag, 23. Januar 2003 15:03
To: General MEMS discussion
Subject: [mems-talk] thermal conductive glue


Mems Group,

I'm looking for a good thermal conductive glue that will bond two
silicon wafers together - and be release after a few operation that
require good thermal conductivity, vacuum compatible, temperature range
between -20 to 125 C.

Thanks,

Greg Miller
KVH Industries
Email: gmiller@kvh.com

_______________________________________________
MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply