Greg, Thermal-conductive pressure sensitive adhesive (PSA) tape would help with this application better than liquid adhesive or glue due to the following advantages: * Good control of thickness variation * Tailored adhesion level to specific bonding substrate * Minimum tension (liquid adhesives usually shrink and introduce tension to substrate) * Easy to use. Never messy. Bond instantly; easily conformable. * Supplied in roll form, allowing higher manufacture efficiency than using liquid adhesive. In this case, you could use a double-face or transfer PSA tape to bond the wafers. We have thermal-conductive PSA tapes, and also have heat release technology where the adhesive loses its tack when heated. Contact me if you need detailed information. Wilson Xia Wilson Z. Xia (Ph.D.) Adhesives Research, Inc. PA 17327, USA. Tel: 1-717-227-3487 wxia@arglobal.com ---------------------------------------------------------------------------- - Mems Group, I'm looking for a good thermal conductive glue that will bond two = silicon wafers together - and be release after a few operation that = require good thermal conductivity, vacuum compatible, temperature range = between -20 to 125 C. Thanks, Greg Miller KVH Industries Email: gmiller@kvh.com