Loren, Have you actually worked with this glass. I have found it to be almost impossible to work with, and expensive. If someone has a lot of experience with this glass please let me know, I would like to learn the "tricks". Thanks, Charles Ellis Auburn University -----Original Message----- From: mems-talk-bounces@memsnet.org [mailto:mems-talk-bounces@memsnet.org] On Behalf Of St.Clair, Loren Sent: Tuesday, January 28, 2003 7:47 AM To: 'General MEMS discussion'; 'sarah.schwab@clarisay.com' Subject: RE: [mems-talk] Photo-definable glass Sarah, Foturan from Schott Corporation is a material that can be patterned using a standard mask aligner (300-320nm) and HF. Craig Wurzel can be contacted at wurzel@schottglass.com if you have any questions about prices. Hope this helps, Loren St. Clair -----Original Message----- From: Sarah Schwab [mailto:sarah.schwab@clarisay.com] Sent: Friday, January 24, 2003 4:38 PM To: 'mems-talk@memsnet.org' Subject: [mems-talk] Photo-definable glass Hello there I am looking for some information on photo-definable glass. Could anyone please help me with the following: Suppliers? Approx cost per wafer 4" diameter - sample quantities? Minimum thickness? Many thanks Sarah _______________________________________________ MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk Hosted by the MEMS Exchange, providers of MEMS processing services. Visit us at http://www.memsnet.org/ _______________________________________________ MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk Hosted by the MEMS Exchange, providers of MEMS processing services. Visit us at http://www.memsnet.org/