Hi,

   We are looking for some information on electroplating thick films of
Indium and Indium Based alloys. Are there any vendors that provide the
electrolytes for plating of indium? We are looking at film thickness in
the order of 5-6 microns.

  Also, is it possible to etch Indium? If yes, any suggestions on
possible etchant are welcome.


Thanks and looking forward to responses,