Hello Yair, I think that it is necessary the use of an adhesion promoter because the Pyralin has bad adhesion properties. The adhesion promoter that I use for the PYRALIN 2555 is the VM 651 from HD MicroSystems. I recommend you to contact with HD MicroSystems. Best regards, Isabel. -----Original Message----- From: Yair [mailto:syair@t2.technion.ac.il] Sent: miércoles 19 de febrero de 2003 7:10 To: 'General MEMS discussion' Subject: RE: [mems-talk] my Pyralin is breaking off Hello Isabel, I don't have an adhesion promoter. Isn't there any other way? Thanks in any case, Yair -----Original Message----- From: Rivas, Isabel [mailto:irivas@ceit.es] Sent: Monday, February 17, 2003 4:58 PM To: General MEMS discussion Subject: RE: [mems-talk] my Pyralin is breaking off Hello Yair, Do you apply an adhesion promoter before the Pyralin deposition?. Best regards. Isabel Rivas Guerrero irivas@ceit.es CEIT, Microelectronic section Pº Manuel Lardizabal Nº 15 San Sebastian (Spain) -----Original Message----- From: Yair [mailto:syair@t2.technion.ac.il] Sent: jueves 13 de febrero de 2003 12:58 To: mems-talk@memsnet.org Subject: [mems-talk] my Pyralin is breaking off Hello, I'm using Pyralin 2555 (1:1), ~3um thick, as a dielectric thin film. After photolitogrphy and development, I want to remove the photoresist (AZ2020) with Acetone, but the Pyralin is peeling off my substrate as well (it is not cured yet). Can anyone recommend me something about that? Thanks a lot, Yair Gannot, Process Engineer Wolfson Microelectronics Research Center TECHNION - ISRAEL INSTITUTE OF TECHNOLOGY Technion City, Haifa 3200, Israel Tel- +972-4-8293291 _______________________________________________ MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk Hosted by the MEMS Exchange, providers of MEMS processing services. Visit us at http://www.memsnet.org/ _______________________________________________ MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk Hosted by the MEMS Exchange, providers of MEMS processing services. Visit us at http://www.memsnet.org/