Our Fab offers Low Stress Nitride films at reasonable cost on 4", 5", and 6" wafers. Please contact our Sales Dept. at tdriver@shipley.com or me directly at nricks@shipley.com to receive a quote. Neal Ricks Maximiliano Fischerwrote:Dear MEMS Specialists, I really appreciate if you could help me find data on residual stresses left in Silicon Nitride layers on usual and hi-quality wafers. For our research, we would need to find very-low-stress nitride-layered wafers or methods to create them by our own. Prices, availability and literature are welcome. Thanks! -- _________________________________________________ Maximiliano Fischer Eng MSc Aero & Astro CNEA - UNSAM MEMS Group _______________________________________________ MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk Hosted by the MEMS Exchange, providers of MEMS processing services. Visit us at http://www.memsnet.org/ --------------------------------- Do you Yahoo!? Yahoo! Tax Center - forms, calculators, tips, and more