************************* Reply Delimiter ***************************** Suggest you contact: Lufran, Inc. 10200 Wellman Road Streetsboro, Ohio 44241 Telephone: (216) 655-9797 Telefax: (216) 656-3500 Their wet chemical etch product line is known as the "superbowl" series of products. Best regards, Ed Kolesar +++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++ Edward S. Kolesar, PhD. P.E. W.A. Moncrief Professor of Engineering Texas Christian University Department of Engineering Electrical Engineering Laboratories Campus Box 298640 2800 South University Drive Fort Worth, TX 76129 Internet E-mail: kolesar@zeta.is.tcu.edu Telephone: (817) 921-7722 ext. 6226 (Direct) (817) 921-7126; 7677 (Secretary) TeleFAX: (817) 921-7136; -7704; -7333 +++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++ ************************** End of Reply ********************************* We are planning to modify our current KOH-etching equipment. Our etcher is just for water-circulating bath, so it isn't so good for etching of silicon using KOH soluton. So we are looking for other baths which are commercially made. Desired spec is as follows : - Operation Temperature 40-80 degree C - Homogeneous distribution of temperature - Condenser which can maintain etchant at constant concentration Optional : Capability of running under ultrasonic sound Could any of you tell me a equipment or providers that sell this etching bath ? Seong-Hyok Kim Lab. for MiSA #301-1104, School of Elec. Eng., Seoul National University, San 56-1 Shillim-dong, Kwanak-gu, Seoul 151-742 Korea Fax : +82-2-873-9953 E-mail : popinjay@plaza.snu.ac.kr WWW : http://plaza.snu.ac.kr/~micro From ROLAND A. LEVY, MATERIALS SCIENCE, (201) 596-3561 Mon Jul 14 16:10:24 1997 To: mems@isi.edu Subject: Sputtering System From: "ROLAND A. LEVY, MATERIALS SCIENCE, (201) 596-3561" Date: Mon Jul 14 16:10:24 1997 Lines: 6 There was a recent inquiry from an organization seeking a sputtering system with load lock and substrate heating capabilities. Should that organization be still interested in such a system, they should contact me because there may be one available. R. Levy