durusmail: mems-talk: Photopatterning
Photopatterning
Photopatterning
David Nemeth
2003-03-10
We tend to attach the wafer to be patterned to another wafer using black
wax.
You won't get as good coverage as on a flat wafer, but play around with spin
speeds and resist viscosity.

David Nemeth

-----Original Message-----
From: mems-talk-bounces+nemeth=sophiawireless.com@memsnet.org
[mailto:mems-talk-bounces+nemeth=sophiawireless.com@memsnet.org]On
Behalf Of sandhya sandhya
Sent: Tuesday, February 25, 2003 5:56 PM
To: mems-talk@memsnet.org
Subject: [mems-talk] Photopatterning



Hello

I am sandhya, a research student . Can ,anyone say me how to apply
photoresist(spin) on a wafer having holes in it and pattern them. we are
using SPR 200 series positive resist.

Thanks

sicerely,

Sandhya





---------------------------------
Do you Yahoo!?
Yahoo! Tax Center - forms, calculators, tips, and more
_______________________________________________
MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply