Hi all,

I had aluminum electrodes on a piezoelectric zinc oxide layer for my
devices. I was planning on using gold electrodes instead and was
wondering if anyone has had any experience with it. I'm not sure if
there is problem with gold maybe not attaching well to the zinc oxide.

Thank you!
Shweta Humad
Shweta@ece.gatech.edu