C4F8 etchant
C4F8 etchant
BobHendu@aol.com
2003-04-03
Anupama:

Do you have the ability to add some CF4 to your plasma ash tool? Try using a
96:4 ratio of CF4:O2 at 100 watts for 5 minutes. You might have to experiment
with time to get best results but if you are dealing with an inorganic residue
of some sort it should take it off. Pressure around 250 mtorr. Bob Henderson