Dear Dr. Shekhar Bhansali, I have several papers on modeling and Non-linear FEM of SMA. My SMA-CAD system can analize two dimensional distribution of stress, strain and transformation for the shape memory effect and pseudo-plastic deformation. If you are interested in these articles, please let me know your address and Tel/Fax. Best regards, Koji Ikuta At 5:38 PM 97.7.28, Shekhar Bhansali wrote: > Dear Colleagues, > > I'm looking for references on modelling pseudo-plastic deformation of near > equi-atomic TiNi SMA thin film. > > Any feedback and comments on the feasibilitiy of the exercise and > suggestions are welcome. > > > Shekhar Bhansali *************************************************** Koji Ikuta ikuta@mech.nagoya-u.ac.jp (Biomedical Micro Mechatronics Lab.) TEL: +81 52 789-5024 FAX: +81 52 789-5027 Department of Micro System Engineering School of Engineering Nagoya University Furocho, Chikusa-ku, Nagoya 464-01, JAPAN ***************************************************