Try polyimide. There are photosensitive or unphotosensitive polyimide. --- kduncan@intellite.com wrote: > Hi. > I am looking for a dialectric coating to deposit on > a gold pad array. I > thought about parylene, but it is not cost > effective. Is there possibly > some spin on glass or something of the sort that > does not have to bake at > 400+? > Thank you, > Kelly > > -- > > _______________________________________________ > MEMS-talk@memsnet.org mailing list: to unsubscribe > or change your list > options, visit > http://mail.mems-exchange.org/mailman/listinfo/mems-talk > Hosted by the MEMS Exchange, providers of MEMS > processing services. > Visit us at http://www.memsnet.org/ __________________________________________________ Do you Yahoo!? Yahoo! Tax Center - File online, calculators, forms, and more http://tax.yahoo.com