Not entirely true. There is a group at CERN headed by Fabio Sauli that regularly wet etches Dupont polyimide foils to make radiation detectors. Search Nuclear Instruments and Methods (an Elsivier Pub.) for GEMs (Gas Electron Multipliers). If you the reference maybe you could share them with us. -Mike >>> fnadi@yahoo.com 04/14/03 09:57AM >>> Is it cured or not? If cured not much can be done, and if it is not you can not etch it, only strip it. Do you mean you want to pattern PI with some other masking material and then wet etch it? --- Shadyar Farhangfarwrote: > Dear All, > > Does anybody happen to know about the wet-etching of > polyimide? Is there any "standard" etchant to wet-etch > polyimide layers? > > Appreciating any hint, > Sh.Farhangfar > > __________________________________________________ > Do you Yahoo!? > Yahoo! Tax Center - File online, calculators, forms, and more > http://tax.yahoo.com > > _______________________________________________ > MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list > options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk > Hosted by the MEMS Exchange, providers of MEMS processing services. > Visit us at http://www.memsnet.org/ __________________________________________________ Do you Yahoo!? Yahoo! Tax Center - File online, calculators, forms, and more http://tax.yahoo.com _______________________________________________ MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk Hosted by the MEMS Exchange, providers of MEMS processing services. Visit us at http://www.memsnet.org/