Shay Kaplan
2003-04-15
Try BCB is is polyimide like but doesn't absorb water.



Likun Zhu wrote:

> Try polyimide. There are photosensitive or
> unphotosensitive polyimide.
> --- kduncan@intellite.com wrote:
> > Hi.
> > I am looking for a dialectric coating to deposit on
> > a gold pad array.  I
> > thought about parylene, but it is not cost
> > effective.  Is there possibly
> > some spin on glass or something of the sort that
> > does not have to bake at
> > 400+?
> > Thank you,
> > Kelly
> >
> > --
> >
> > _______________________________________________
> > MEMS-talk@memsnet.org mailing list: to unsubscribe
> > or change your list
> > options, visit
> >
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> > Hosted by the MEMS Exchange, providers of MEMS
> > processing services.
> > Visit us at http://www.memsnet.org/
>
> __________________________________________________
> Do you Yahoo!?
> Yahoo! Tax Center - File online, calculators, forms, and more
> http://tax.yahoo.com
>
> _______________________________________________
> MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/


reply