wet-etching of polyimide
Robert Dean
2003-04-15
Hello,

Some polymeric materials, such as LCP, can be etched with heated
KOH.  Additionally, even though it is not a wet etch, many polymeric
materials can be etched with O2/Ar RIE, using a simple thin film patterned
metallic mask.

Sincerely,

Robert Dean

At 03:04 PM 4/14/03 -0400, you wrote:
>Not entirely true. There is a group at CERN headed by Fabio Sauli that
>regularly wet etches Dupont polyimide foils to make radiation detectors.
>Search Nuclear Instruments and Methods (an Elsivier Pub.) for GEMs (Gas
>Electron Multipliers). If you the reference maybe you could share them
>with us.
>
>-Mike
>
>
> >>> fnadi@yahoo.com 04/14/03 09:57AM >>>
>Is it cured or not? If cured not much can be done, and if it is not you
>can not
>etch it, only strip it. Do you mean you want to pattern PI with some
>other
>masking material and then wet etch it?
>
>
>--- Shadyar Farhangfar  wrote:
> > Dear All,
> >
> > Does anybody happen to know about the wet-etching of
> > polyimide? Is there any "standard" etchant to wet-etch
> > polyimide layers?
> >
> > Appreciating any hint,
> > Sh.Farhangfar
> >
> > __________________________________________________
> > Do you Yahoo!?
> > Yahoo! Tax Center - File online, calculators, forms, and more
> > http://tax.yahoo.com
> >
> > _______________________________________________
> > MEMS-talk@memsnet.org mailing list: to unsubscribe or change your
>list
> > options, visit
>http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> > Hosted by the MEMS Exchange, providers of MEMS processing services.
> > Visit us at http://www.memsnet.org/
>
>
>__________________________________________________
>Do you Yahoo!?
>Yahoo! Tax Center - File online, calculators, forms, and more
>http://tax.yahoo.com
>
>_______________________________________________
>MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.memsnet.org/
>
>_______________________________________________
>MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.memsnet.org/
reply