Esteban,
Are you using a Dicing saw to make the 10x20m sections ?  If you are
trying another mechanical scribe/break or other- it is likely that the
thin Si is just too fragile to facilitate a clean cut with your method.
Suggest using Diamond Saw Dicing with the 30um wafer on 'tape' to give
it the structural control to allow the cutting. There are several
services that can do this process for you - if you do not have dicing
capability in house.
Regards
Ken

Esteban Broitman wrote:
> Does anybody know how to "cleave" ultra thin Si wafers?
> I need to cut, from ultra-thin (30 microns) Si wafers, substrates of ~
> 10 x 20 mm. I tried to use different kind of diamonds, but I always have
> the same problem: the substrate is not more "flexible", if I try to bent
> it, it cracks in many parts. I suspect that I am generating defects
> during the cutting of the substrates that propagate during the bending.
> Any suggestion?.
> Thanks for the reply to my e-mail: broitman@andrew.cmu.edu
> E. Broitman
> ----------------------------------
> Dr. Esteban Broitman
> Senior Research Associate
> Department of Chemical Engineering
> Carnegie Mellon University
> Pittsburgh,  PA 15213
> Phone: (412) 268-9537
> FAX: (412) 268-7139

Kmbh Associates
47 Rocket Circle
Rancho Cordova, CA 95742  U  S  A
510-714-5055 Efax- 510 217 4421 or 561 658 6136

High Purity Float Zone and Specialty CZ Silicon  for Power, IR and
Mirror Optics, Optoelectronics, MEMS, SOI, and other Semiconductor
applications. Service in SOI, Polishing SSP and DSP.
Quartz, Glass, Pyrex and Borofloat Wafer Supply. Anodic Bonding. SOG, SOS.



reply