Hello Who supplies Parqit, we can not find any supplier of this product. George Steimle University of South Florida Process Development Specialist College of Marine Science Center For Ocean Technology 727-553-3937 Fax: 727-553-3967 E-mail:gsteimle@marine.usf.edu 140 Seventh Avenue South St. Petersburg, Florida 33701-5016 ----- Original Message ----- From:To: Sent: Friday, May 30, 2003 5:58 PM Subject: [mems-talk] Parqit remover > Hello. > I am interested in using Parqit (a photocuring epoxy resin) on oxide films (e.g. TiO2, > SiO2 on Si), but wonder if there is any good remover for it. > Has anyone tried anything for the remover? > Thank you so much for your comment. > > Tetze Hamano > > > _______________________________________________ > MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list > options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk > Hosted by the MEMS Exchange, providers of MEMS processing services. > Visit us at http://www.memsnet.org/ >