Dear colleagues, does anyone have any experience with the surface properties of cured bcb films, such as contact angle with water and other liquids? How hydrophobic is it? Any ideas on how to modify the bcb surface using wet chemistry? -- Nikola Pekas graduate assistant Iowa State University