Both processes build residual stress on thin films. The quantum of stress depends on thickness of the film deposited. Sputter process has high stress even for low thickness films. Stress is less for plated films at low thickness. You need to choose your process based on your application and thickness. Best regards Gautham, Absara Micro Systems