Transene Company manufactures cyanide and sulfite based gold etchants. The traditional cyanide etchant, SG-10, has been used in MEMS applications. Data sheets are available at www.transene.com. Feel free to contact me if you would like additional information. Christopher Christuk Transene Company 10 Electronics Avenue Danvers MA 01923 Tel: 978 777 7860 Fax: 978 739 5640 Email: Christopher@transene.com -----Original Message----- From: LSWANG [mailto:lswang2001@yahoo.com] Sent: Friday, July 11, 2003 6:53 PM To: mems-talk@memsnet.org Subject: [mems-talk] AU electroplating solution Dear MEMS colleagues, Can anyone give me some suggestion of what kind of Au electroplating solution is widely used in MEMS application, I have checked Technic 's website, they have some kinds, but i don't know which one is better. Thanks Best Lisen Lisen Wang Graduate student University of California, Irvine __________________________________ Do you Yahoo!? SBC Yahoo! DSL - Now only $29.95 per month! http://sbc.yahoo.com