durusmail: mems-talk: polysilicon etch back
polysilicon etch back
2003-07-24
polysilicon etch back
BobHendu@aol.com
2003-07-27
You might try chemical mechanical polishing. There is a good company located
in Tempe, Az called Total Fab solutions that can help you out. Ask for Steve
Horowitz. Bob Henderson