Dear collegues: We would like to inquire if any of you have tried to dilute BCB (Cyclotene) available from Dow Chemicals to achieve thinner coatings. Please, advise on the procedure. Thank you very much. Ivan Shubin Research Scientist ECE Department, EBU-1, M.C. 0407 University of California, San Diego La Jolla, CA 92093 ph./fax (858) 534-6570