Dear all, Can anybody suggest an etchant which can etch Pb and resistive to Ag and Si.I wants to etch 6A of Pb on 60A of Ag deposited over Si(100) substrate. Thanks in advance, Sinu Mathew. __________________________________ Do you Yahoo!? Yahoo! SiteBuilder - Free, easy-to-use web site design software http://sitebuilder.yahoo.com