Hello MEMS's Men, I try to make wire bonding on a PZT thin film (with high roughness) with a classical deposition of Cr and Gold on but each time, the layers of Cr and Gold are peeled off. What can I do ? remark : the surface of the PZT film is to small for use silver past. Thanks for your help Eric -- Dr. Eric Bonnotte LIMMS/Kawakatsu laboratory / CNRS/IIS-The University of Tokyo 7-22-1 Roppongi Minato-ku Tokyo 106 JAPAN Tel/FAX : +81-3-3402-9568 Tel/Fax Home : +81-3-3411-5381 E-mail : ebon@cc.iis.u-tokyo.ac.jp