Hi Laurent, Yes, the solvent is propylene glycol monomethyl ether acetate. It is sold by Shipley (Also by us at MicroChem as their distributor) in the U.S. as Type P Thinner. However, just to make clear things muddy, it is also sold as "EC Solvent" by Shipley in Europe. The products are identical. Just be careful because the EC Solvent 11 product sold in the U.S. is NOT THE SAME. It is ethyl lactate. Hope that 's no too much information! Very Best Regards, Rob Hardman 617-965-5511 ext.313 rhardman@microchem.com www.microchem.com Date: Mon, 08 Sep 2003 16:03:58 +0000 From: "laurent gangloff"Subject: [mems-talk] shipley 1805 solvent? To: mems-talk@memsnet.org Message-ID: Content-Type: text/plain; charset=iso-8859-1; format=flowed Hi all, Could anyone tell me what is the solvent use in the 1805 resist from shipley? Thanks. _________________________________________________________________ Hotmail : un compte GRATUIT qui vous suit partout et tout le temps ! http://g.msn.fr/FR1000/9493