Ti or Cr is good choice -----Original Message----- From: Sebastian Sosin [mailto:sebastiansosin@rdslink.ro] Sent: Thursday, October 23, 2003 10:19 PM To: mems-talk@memsnet.org Subject: [mems-talk] what about platinum over silicon dioxide? Do I need an adhesion layer before depositing platinum over silicon dioxide? _______________________________________________ MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk Hosted by the MEMS Exchange, providers of MEMS processing services. Visit us at http://www.memsnet.org/