We can fabricate these masters out of nickel using either X-ray or UV
Lithography.  You may contact me below for questions or a quotation.

Dean Guidry
International Mezzo Technologies, Inc.
guidry@mezzotech.biz
Phone (225) 578-7602
Fax (225) 334-6395
www.mezzotech.biz

-----Original Message-----
From: mems-talk-bounces+guidry=mezzosystems.com@memsnet.org
[mailto:mems-talk-bounces+guidry=mezzosystems.com@memsnet.org] On Behalf Of
Hong Wang
Sent: Friday, October 31, 2003 2:23 AM
To: mems-talk@memsnet.org
Subject: [mems-talk] where to buy master for microchannel fabrication


Dear All,
    We want to do some DNA analysis in microchannels. The channel size maybe
100micro width, 20-50 micro depth and 1cm length. We don't want to
fabrication master by ourself. Does anyone know where can we buy some? Any
proper material of master suitable for PDMS channel fabrication is fine.
Thank you. Hong _______________________________________________
MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services. Visit us
at http://www.memsnet.org/


reply