durusmail: mems-talk: Re: Polyimide info wanted
Re: Polyimide info wanted
1995-09-22
1995-09-22
1995-09-23
1995-09-26
Re: Polyimide info wanted
Gang Lin
1995-09-22
>
>
> I'm looking for information on the use polyimide as an interlayer
> insulator.  I got some info from the Berkeley Microlab homepage which
> talks about a specific product called "PIX L110".  Does anyone have any
> experience in the use of this product?  I'd appriciate any information on
> where I can purchase this product, application, curing process, etc...
>
> Thanks in advance.
>
> Y. M. Desta
> LSU mSET, Dept. of Mech. Engr.
>
If you email me your fax number, I can fax a page of product brochure, which
has PIX L110 on it, to you.

Dr. G. LIN
IfM, Louisiana Tech University
lingang@engr.latech.edu


reply