You should be fine. If there are any pin holes in the gold then the HF will find a way to the substrate but if your coating is uniform you should have no problems. Tres -----Original Message----- From: li Yu [mailto:yuli_st1234@yahoo.com] Sent: Sunday, February 15, 2004 9:14 PM To: mems-talk@memsnet.org Subject: [mems-talk] Does concentrated HF etch Au I want to put a wafer with 2000A Au in 49% HF for 30 minute, Is that Ok? Thanks in advance. Lili --------------------------------- Do you Yahoo!? Yahoo! Finance: Get your refund fast by filing online _______________________________________________ MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk Hosted by the MEMS Exchange, providers of MEMS processing services. Visit us at http://www.memsnet.org/