adhesion of oxide to evaprated chromium
JOHNSON,MARK (HP-Corvallis,ex1)
2004-02-23
Anna,
I think you will find that chromium does form an oxide. There are several
references in the literature related to this, since it is used as a coating
metal for SEM.
Mark
-----Original Message-----
From: mems-talk-bounces+mark.d.johnson=hp.com@memsnet.org
[mailto:mems-talk-bounces+mark.d.johnson=hp.com@memsnet.org]On Behalf Of
Anna Ohlander
Sent: Saturday, February 21, 2004 10:26 AM
To: mems-talk@memsnet.org
Subject: [mems-talk] adhesion of oxide to evaprated chromium
Hello,
Does anybody know anything about the adhesion of PECVD si oxide to
evaporated chromium? I've read that Chromium doesn't form a native oxide in
room temperature. What's the secret behind it's potential as an adhesion
layer?
/ Anna
_________________________________________________________________
Hitta rätt på nätet med MSN Sök http://search.msn.se/
_______________________________________________
MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/