Hello everyone,

I am going to RF Sputter lead-zirconate-titanate (PZT)
onto platinized Si substrates. The problem I am having
is of Pb contamination, and so the cleanroom staff
here is very reluctant to allow any Pb inside. They
are afraid that Pb will be poisonous to users in the
clean room. Has anyone faced a similar problem before?
If so, please help me out here.

Thanks.