Hi,

 I would like to know what could be the allowed temperature tolerance for the
KOB bath used for etching silicon, as we cannot maintain the bath exactly at one
particular temperature as it keeps fuctuating around 2-3 degrees.
I would really appreciate if you could reply.

Thanks,
dhanamjaya