Dear friends, I have spin coated a thin Layer of PMMA over Quartz block in my laboratory. I want to measure the film thickness and Refractive index, can anybody suggest some way of doing it. Your help will be heartly appreciated. regards Aashish Singh Project Associate Department of Physics Indian Institute of Technology, Delhi New Delhi-16 INDIA