> everybody! I want to measure the deflection of a membrane, and the magnitude of the deflection is about 30um. > > Could you give me some advice on the work? Read the articles by Artur Degen, University of Kassel, in J.Vac.Sci.Technol or Microelectronic Engineering or other journals. Best regards B.E. Volland