AZ4620 Removal after High temperature Bake
2005-03-09
2005-03-10
2005-03-14
AZ4620 Removal after High temperature Bake
Russell Davies
2005-03-14
Hi,
Rohm & Haas (formally Shipley) have a very good range of polymer &
photoresist strippers which may work. Otherwise you could use a release
layer based on PMGI or LOR from Micro Chem Corp.

Regards,

Russell A Davies