Does anyone have a method to repeatedly clean a combination silicon
nitride and oxide surface of organics?  Piranna and Nitrated Piranna
appear to damage the nitride and plasma cleaning takes to long to remove
the organics.

I need to be able to use this proceedure numerous times without etch or
oxidizing the layers.