Hello It seems from etching experiments (in di capacitive plasma chamber), that I am not making good enough contact between the substrate and the bottom electrode plate. Is there a economical feasible way for doing so? I think that using an adhesive might be a good idea to stick the wafer directly to the aluminum electrode plate. But it has to be both thermally and electrically conductive, although electrically is more important. And it will has to be able to withstand the high temperatures of the plasma (not sure what the range is). Any recommended products to try? thanks, Xiaoyu