Dear all, We have Su-8 2025, which is 25um thick at 4000rpm. We want to gain thickness of 40um so we tried double-spin. We found that edge bead is very serious and the surface is not so smooth as single spin. Anyone knows any method to enhance its performance, such as, whether we should bake it after each spin, and remove edge bead after each spin? What is the usual solvent used to remove Su8 edge bead? And how? cheers Jiang Ziling