Hi Everyone:

I am trying to measure UNCD (diamond) thickness using a SEM
by looking at the cross sectional area.  I am using a
diamond tip to cut my samples but I am not able to get a
clean cross-sectional area.  I was just wondering if anyone
has any advice or recommendation.

Thanks in Advance;

ej
==========================================================================