Hi-

I was wondering if it is possible to do some sort of lift off process for
creating and oxide mask (2-3 um thick). I found wet etch do be terrible for
accuracy and we have been experiencing problems with our plasma etch
process for some time.

Just looking for an alternative. I am told it can not be done, but I figure
maybe some one may have tried it.

Thanks
Pete