Make your mask with Ni. Brent "R Zhang, Electrical & Electronic Engineering" wrote: > Dear all, > I try to get some material which can prevent from SF6 dry etching for > at least half an hour. And also it can be coated on the Si substrate or > itself can be as a plate. if you know, could you please introduce it to me?