What kind of epoxy are you using? Duh? Original Message: ----------------- From: Mohammad Najmzadeh najmzade@student.chalmers.se Date: Mon, 4 Sep 2006 21:53:23 +0200 (CEST) To: mems-talk@memsnet.org Subject: [mems-talk] dissolving cured epoxy glue Hello, I have attached some silicon sensors to an aluminium setup with epoxy glue and now I want to disconnect them. I am looking for a way to dissolve this cured epoxy glue. Heating of it for 3 hours on a hot plate with 200-300 degree C was one option to dissociate that glue but that was not successful. Please inform me if you know anything about it. Kind Regards, Mohammad Najmzadeh