Hi all, I am trying to put down 300~500nm Au film on Si dioxide as electrodes, and I am just wondering what kind of adhesive layer (needs to be electrically conductive) should I deposit before Au to improve the adhesion? And anyone has some good thoughts about how to pattern the gold electrode (as well as the adhensive layer)? Will regular lift-off work? Thanks much, JJ Hu