Hi all, Now we are doing ECES experiment using AMMT's single channel potentiostat and find some strange problems. When we did IU experiment, we found that the voltage scan stoped in 1.2V even if we set the scan range from -3 to 3V. Does anyone have experience on this and succeed in ECES experiment using AMMT's potentiostat? Any help is greatly appreciated. Regards, Gang Li