Try stripping optical fibers. Shay -----Original Message----- From: mems-talk-bounces@memsnet.org [mailto:mems-talk-bounces@memsnet.org] On Behalf Of Po-Jui Chen Sent: Monday, September 25, 2006 9:14 PM To: mems-talk@memsnet.org Subject: [mems-talk] glass rods Hi, I'm looking for glass rods in small diameters (150-300um). They have to be made out of glass or silica but without any reinforcements. Please advise where I can get some of them.