There is a process called electroless nickel plating. Electrolytes can be bought at SURTEC or ATOTECH. You just dip your Substrate into the solution and the plating occurs at the surface. It works with copper to! Both need a slightly conductive layer to get good results. Maybe you have to evaporate a conductive layer (Copper would be the best, or PD seeds or graphite, or oxidizing) on top of your substrate first. Good luck! Sebastian -----Original Message----- From: mems-talk-bounces@memsnet.org [mailto:mems-talk-bounces@memsnet.org] On Behalf Of madhav rao Sent: Thursday, November 02, 2006 7:48 PM To: General MEMS discussion Subject: [mems-talk] Nickel electroless Plating!! Hi All, I am not able to find a simple way of doing electroless Nickel plating on PMMA patterned silicon wafer. Can any one provide me any PDF file or any procedure to do Electroless Nickel plating.