durusmail: mems-talk: temporary bonding solutions
temporary bonding solutions
2006-11-05
2006-11-06
2006-11-06
2006-11-07
temporary bonding solutions
Barrie VanDevender
2006-11-07
This should work fine for 250um thick material.


-----Original Message-----
From: mems-talk-bounces@memsnet.org [mailto:mems-talk-bounces@memsnet.org]
On Behalf Of Mathieu Foquet
Sent: Monday, November 06, 2006 12:28 PM
To: Sebastian Sosin; mems-talk@memsnet.org
Subject: RE: [mems-talk] temporary bonding solutions

Revalpha thermal release tape is one idea. (Nitto Denko)

-----Original Message-----
From: mems-talk-bounces@memsnet.org
[mailto:mems-talk-bounces@memsnet.org] On Behalf Of Sebastian Sosin
Sent: Sunday, November 05, 2006 7:54 AM
To: mems-talk@memsnet.org
Subject: [mems-talk] temporary bonding solutions

I am looking for a temporary bonding solution that can be removed
without solvents (heat, UV.). It may be glue or adhesive tape. Does
anyone know any products like this?
reply