hi, guys:
       I need some wafter boat which can be immersed into the SU8 developer. I
have some which came with the wafer I bought. But I'm not sure which material
are they made of, or can they resist the SU8 developer? Is there anyone who has
experience on this, or do u know where to buy such kind of process boats, any
suggestion will be appriecated. thx